Cooperating with Petroleum University and Sinopec Gaoqiao Branch, we spent 3 years to develop JT x series Arene extender oil. Tested and compared by Sinopec Gaoqiao Branch with the imported Arene extender oil. The technical indexes of our products are the same with the Japanese products, and the technical indexes of its finished products are the same with the finished products made by Japanese Arene extender oil. Especially, its tension on 300% elongation, tensile strength, elongation on break, viscosity and hardness just like the Japanese products. It can be used as substitute of import products to produce SBR.
Our rubber oil & extender oil are made of domestic and imported materials, we have good material supplier. Taking based oils with medium viscosity as materials, strictly controlling the refining condition of furfural and operational conditions of production, we now can offer you qualified products.
Feature:
1, good compatibility with rubber; 2, low volatility; 3, easy to process; 4, good stability; 5, no bad effect; 6, good emulsification ; 7, good bending performance; 8, good tensile strength, elongation on break and shear strength. We also offer other specification for you
JT-X series rubber oil production unit:
Specification:
Item\Quality index\ Model |
JT-1 rubber oil |
JT-2 rubber oil |
Test method |
Kinematic viscosity (98.89℃) |
14-18 |
18-25 |
ASTMD445-04e2 |
Density(20℃),kg/m3 |
0.893-0.95 |
0.92-0.98 |
ASTMD4052-96(2002)el |
Flash point((open)℃≥ |
190 |
200 |
ASTMD92-05a |
freeze point ℃≤ |
+5 |
+13 |
GB/T510-1983 |
Refractive index (20℃) |
1.48-1.52 |
1.50-1.55 |
ASTMDl218-02 |
Moisture ,% |
trace |
trace |
ASTMD95-05el |
Loss on evaporation (163℃/3h)≯ |
1 |
1 |
Loss on Heating@163℃,3h |
Carbon structure% |
|
CA |
8-12 |
10-16 |
ASTMD2140-97 |
CN |
report |
report |
ASTMD2140-97 |
CP |
report |
report |
ASTMD2140-97 |
|